之前,如果没有 ?> 就直接放最后)===== // 1) Google Search Console 验证标签 add_action( 'wp_head', function () { echo '' . "\n"; }, 1 ); // 2) 匿名访问的 HTML 加 CDN 缓存头(浏览器不缓存,CDN 缓存 1 小时) add_filter( 'wp_headers', function ( $headers ) { if ( is_admin() || is_user_logged_in() ) { return $headers; } $headers['Cache-Control'] = 'public, max-age=0, s-maxage=3600, stale-while-revalidate=86400'; return $headers; }, 20 ); // ===== 粘贴结束 ===== Aluminum Die Casting Design Guide | Walls, Draft & Cost

Dongguan, Guangdong, China · ISO 9001 quality system

Guide

Aluminum die casting design guide

Design rules for aluminum die casting: alloy choice, wall thickness, draft, ribs, bosses, porosity, machining stock and cost drivers.

  • ISO 9001 quality system
  • Quotes within hours
  • Prototype to production

Overview

Start with the process, not the part

Die casting makes sense when the geometry is complex, the volume is repeatable and the part can be ejected from a steel mold. If the design needs undercuts in three directions or a wall thinner than the alloy can fill, the tooling will be complicated and the scrap rate will show it.

This guide covers the decisions that most often determine whether a casting is cheap, difficult or impossible. It is written for product engineers, not toolmakers, and it assumes aluminum.

Alloy

Alloy quick reference

AlloyStrengthCorrosionMachinabilityTypical use
A380 / ADC12GoodModerateExcellentHousings, covers, general parts
A360GoodBetterGoodOutdoor and wet environments
A413ModerateGoodGoodThin-wall and intricate parts
B390High wear resistanceModerateModerateWear plates and abrasive service

Walls

Wall thickness: uniform beats thin

Thin walls cool quickly and can be strong, but they also fill less easily and are harder to machine. The bigger problem is variation: a thick section next to a thin one cools at a different rate, and that is where shrinkage porosity appears.

Aim for uniform walls, and transition gradually when thickness has to change. A common starting range for aluminum die casting is about 2 to 4 mm, but the correct value depends on part size, alloy and flow length.

  • Keep walls as uniform as possible
  • Avoid thick masses next to thin sections
  • Transition thickness gradually
  • Consider flow length from the gate
  • Leave machining stock only where needed

Draft and radii

Draft, radii and ejection

Draft is the taper that lets the part release from the mold. Without it, the part drags, scratches or sticks, and the operator compensates with release agent and force. A typical starting point is 1 to 2 degrees on walls, more on textured surfaces.

Internal radii reduce stress and improve flow. Sharp corners are stress concentrators and are difficult to fill. Ejector pins need flat, non-cosmetic surfaces to push against.

  • 1 to 2 degrees of draft on walls
  • More draft on textured surfaces
  • Generous internal and external radii
  • Ejector pins on hidden surfaces
  • Avoid sharp inside corners
  • Design gates and overflow space

Features

Ribs and bosses

Ribs add stiffness without adding a thick wall. Bosses create mounting points, but they are also masses that cool last. A boss with a thick wall will pull a sink mark on the opposite face or create porosity at the junction.

Use gussets to support bosses, keep boss walls close to the nominal wall thickness, and put a small radius at the base instead of a sharp step.

  • Rib thickness below nominal wall
  • Boss walls close to nominal thickness
  • Gussets instead of sharp junctions
  • Avoid isolated masses
  • Allow for core pins
  • Check machining access

Tooling complexity

Undercuts and sliders

An undercut that blocks ejection needs a slider or a lifter. Every slider adds tooling cost, maintenance and cycle time. If the undercut is cosmetic, consider a secondary operation or a design change instead.

Discuss undercuts with the toolmaker before the design freeze. Moving a snap feature by a few millimeters can remove a slider entirely.

Porosity

Porosity and leak paths

Porosity is a fact of die casting. The goal is to keep it out of critical sections and away from sealing surfaces. Gate position, wall uniformity, venting and shot parameters all influence where porosity ends up.

For parts that must hold pressure, design the seal away from the gate and the last-filled area, and plan leak testing into the validation. Machining through a porous section can open a leak path; sometimes it is better to cast a boss and machine it.

If the part must be leak-tight, tell the supplier at quoting. It changes the tool design and the process window.

Finish and machining

Surface finish and machining stock

As-cast surfaces have a texture that depends on the mold finish. Cosmetic parts need a polished or textured mold, and that cost belongs in the tooling quote. Functional surfaces are usually machined.

Leave machining stock on faces that will be cut. The amount depends on the casting tolerance and the fixture. Too little stock leaves defects; too much adds cycle time and cost.

  • Specify cosmetic vs functional surfaces
  • Agree mold texture
  • Leave stock on machined faces
  • Protect sealing faces
  • Plan masking for coatings
  • Check flatness after machining

Cost

Cost drivers in a casting quote

DriverEffect
Part size and projected areaPress size and cycle time
Wall thicknessFill time, cooling and strength
Sliders and liftersTooling cost and maintenance
Cavity countTooling cost vs cycle time
Machining stockCycle time and tool wear
Cosmetic requirementsMold finish and polishing
Leak test / X-rayInspection cost per part

Checklist

A short DFM checklist

Before you send a casting RFQ, check the walls, draft, radii, undercuts, ejector surfaces and machining stock. Mark the surfaces that matter and state the annual volume. Those six facts let a supplier quote the tool and the part properly instead of guessing.

If you want a second opinion on a design, send the model. We will mark the features that drive tooling cost and suggest changes that keep the function.

  • Uniform wall thickness
  • Draft on all walls
  • Radii at internal corners
  • Under cuts and sliders identified
  • Ejector pin locations
  • Machining stock and datums
  • Cosmetic surfaces marked
  • Annual volume and launch date

FAQ

Questions buyers ask before the first order

What is the minimum wall thickness for aluminum die casting?

It depends on part size and alloy, but a practical starting point is around 2 to 3 mm for many parts. Thin walls need good flow and can be difficult to fill and machine.

How much draft is needed?

About 1 to 2 degrees on walls is typical, with more on textured or deep surfaces. The toolmaker will confirm the final value.

Can die castings be leak-tight?

They can be, with the right gate and process design plus leak testing. Porosity is always present to some degree; the design has to keep it away from sealing features.

Should I cast or machine the threads?

Usually machine them. Cast threads are possible but less precise; machining gives better control of the class and the fit.

How much machining stock should I leave?

Enough to remove casting variation and surface defects, but not so much that cycle time suffers. The supplier should confirm the allowance based on the casting tolerance.

Start a project

Send your drawings. Get a quote in hours.

Upload CAD files or send a sketch with material, quantity and finish. Our engineers reply with pricing, DFM notes and a lead time, usually within one business day.

Request a quote Email engineering

Typical reply: within 1 business day

Call Get a quote